Conventional

Mild Steel

Pipe Welding

Low Hydrogen

Stainless Steel

Cast Iron

Hard Facing

Cutting & Gouging

Low Heat Input Welding Alloys

For Steels

For Disimilar Steels

For Cast Iron

For Stainless Steels

For Copper & Non Ferrous Alloys

For Nickel & Nickel Alloys

For HardSurfacing & Wear Resistant

For Cutting & Gouging

CCMS Wires


MIG/TIG Wires


Flux Cored Wires


SAW Wires & Flux


Welding Rectifier


Welding Transformer


Silver Brazing Wires


MIG/MAG Machines

Sunday, September 05, 2010

Enquiry Cart (0) items

View Cart | Check Out

Home

The Company

Products

Process

Network

Feedback

Contact Us

Products Application

General Welding Safety

Storage of Welding Electrodes

I.S Classification (IS 814-04)

AWS-Classification

General Conversion Table

Properties of Metals & Alloys

En Series & Properties

Standard Casting Specification

Welding Defects & Remedies

MSDS



info@rasielectrodes.com

Keywords

e.g. Nickel based electrode

Select your Choice

 

Conventional  >>  Hard Facing Electrodes  >>  RASI HF MANG 13

HARD FACING ELECTRODE
RASI HF MANG - 13
AUSTENITIC Mn STEEL

CHARACTERISTICS
RASI HF MANG -13 is a low hydrogen type hard facing electrode yielding 12% to 14% Manganese in the weld deposit. The weld deposits which display excellent resistance to impact in combination with corrosion.

EXCLUSIVE FEATURES
 Soft and Stable arc
Good impact resistance
12 - 14% Maganese deposit.

APPLICATIONS

Used on a wide range Similar and dissimilar steels, such as joining of austenitic maganese steel to themselves and to ferritic steels. For welding of heat treatable alloy steels for fabrication welding, maintenance and reclamation of worn out parts, both for buffer layer and hard facing in mining , cement, steel, power plant, earth moving machinery and welding 14% Manganese steels etc.

Welding Current and Packing Data : AC / DC(+)
Dia (mm) 3.15 x 450 4 x 450 5 x 450 Hardness
Current (A) 100-140 140-180 170-230 As Welded :200BHN
Pieces/Pkt 45 30 20 Work hardness 500-550 BHN
Pkts/Box 8 8 8

STORE DRY : If exposed and damp, heat the electrode at 300oC for one hour maintain above 100oC and use.

HINTS ON WELDING
No preheating necessary for mild steel jobs
Clean the weld area thoroughly free of any foreign matter
Use low current
Short arc and stringer bead.

Add to Enquiry Cart | View Cart (0)